Corrected offset in thickness is (min ) may be wrong , it might have a chance to affect on a quality of job. pl be very of insist to ASME committy .
Regards,
RK Vichare
----- Original Message -----
From: Raghuram Bathula
To: Materials-Welding
Sent: Mon, 18 Jul 2011 10:48:15 +0530 (IST)
Subject: [MW:11779] Maximum Allowable Offset In Welded Joints // ASME SEC VIII div2 //
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Regards,
RK Vichare
----- Original Message -----
From: Raghuram Bathula
To: Materials-Welding
Sent: Mon, 18 Jul 2011 10:48:15 +0530 (IST)
Subject: [MW:11779] Maximum Allowable Offset In Welded Joints // ASME SEC VIII div2 //
please refer the attchement, seems to be a typo error while revising code in 2007, they may correct it in the next edition
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments