Skip to main content

Re: [MW:11800] FW: hydraulic test pressure of Pipe.

Hi,
For Stainless stell pipes,(Ex.,SA312) please find below the Code Extraction od SA312. It is the option of the manufacturer unless otherwise purchaser specified to do Hydroatatic test.
 

12. Hydrostatic or Nondestructive Electric Test

12.1 Each pipe shall be subjected to the nondestructive

electric test or the hydrostatic test. The type of test to be

used shall be at the option of the manufacturer, unless

otherwise specified in the purchase order.

12.2 The hydrostatic test shall be in accordance with

SpecificationA 999/A 999M, unless specifically exempted

under the provisions of 12.3.

12.3 For pipe whose dimensions equal or exceed NPS

10, the purchaser, with the agreement of the manufacturer,

may waive the hydrostatic test requirement when in lieu

of such test the purchaser performs a system test. Each

length of pipe furnished without the completed manufacturer's

hydrostatic test shall include with the mandatory markings

the letters "NH."

12.4 Nondestructive Electric Test:

Nondestructive electric tests shall be in accordance with

Specification A 999/A 999M.

 

16. Certification

16.1 In addition to the information required by Specification

A 999/A 999M, the certification shall state whether

or not the material was hydrostatically tested. If the material

was nondestructively tested, the certification shall so state

and shall show which standard practice was followed and

what reference discontinuities were used.

 
For Alloy Tubes (Ex.,SA213) Please find below the Code Extraction of SA213
 

10. Hydrostatic or Nondestructive Electric Test

10.1 Each tube shall be subjected to the nondestructive

electric test or the hydrostatic test. The type of test to be

used shall be at the option of the manufacturer, unless

otherwise specified in the purchase order.
 
 
 
Thanks & Regards,
 
 


(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 7/18/11, subrata das <sdas@pkgroup.org> wrote:

From: subrata das <sdas@pkgroup.org>
Subject: [MW:11794] FW: hydraulic test pressure of Pipe.
To: materials-welding@googlegroups.com
Date: Monday, July 18, 2011, 11:45 AM

Dear Experts

Generally hydraulic test pressure of Carbon Steel pipes are defined by SA-53. But what about the Stainless Steel & Alloy Steel pipes ? Can anyone reply please.  

 

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...