Saturday, July 16, 2011

Re: [MW:11759] PQR testing with RT & UT

Abhishek,

Since, FCAW is more susceptible to lack of side wall fusion, RT  may not detect such a defect and hence  UT is the best suited method of NDT to detect LOF.

Nandeesh


--- On Fri, 15/7/11, ABHISHEK GHOSH <ghoshabhishekmech@gmail.com> wrote:

From: ABHISHEK GHOSH <ghoshabhishekmech@gmail.com>
Subject: [MW:11740] PQR testing with RT & UT
To: materials-welding@googlegroups.com
Date: Friday, 15 July, 2011, 3:57 PM

Dear Experts, 

Why UT along with RT is performed while qualifying a procedure with FCAW welding, At which clause in ASME 9 it is mentioned that UT & RT both has to be performed ?? 

With regards. 

AG

--
ABHISHEK GHOSH
FAHAHEEL, KUWAIT
MOB: (00)965-65772043

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...