Dear sandeep,
 
However as mentioned by Dinesh, voltage, current & travel speed as the important factors afftecting the heat input.
as per my past experience related to SMAW we used to control these factors by increasing the travel speed thereby resulting in good impact values. I am not sure about GMAW, whether this method can be applicable.
Another factor which effects the energy value is the choice of consumables.
 

Regrads,

Yusufkhan. M. Pathan

Engineer-Quality

Air Liquide Engg (IND) Pvt.Ltd.

Email to : yusufkhan.pathan@airliquide.com

Cell:(+91) 8008804165



 
On Wed, Jul 6, 2011 at 12:29 PM, sandy <sandeepdhiman63@gmail.com> wrote:
Dear All
How we can get better impact values in HAZ with GMAW process in non
alloyed carbon steel?
like with multi pass welding.
Please provide your valuable ideas.

Regards
Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...