Skip to main content

Re: [MW:11742] Clarification of PQR/WPS in FCAW process

Hi,
Find below the answers as marked in Red color.
  1. In FCAW proces PQR , Electrode AWS no. E71-T-1C is used. But in WPS E71-T-1 is mentioned. Whether its ok? - OK
  2. PQR in FCAW qualifies 3G position of 27mm plates as per ASME SEc.IX and API-650. What is qualification of position in WPS for 3G whether its ALL POSITION or only 3G postion? - As per ASME Sec.IX, Position is not an essential variable for WPS.WPS qualified in any position can be used for all position.
  3. The WPS is to be used for structural activies. ie. as per AWS D1.1. But in WPS also mentioned reference code as ASME sec.IX and AWS D1.1. - If your construction Code is AWS then the WPS shall be qualified with AWS Code only.You please review your WPS/PQR Whether it has been qualified with AWS or not.if the test and variables are meets the AWS limitation then you just revise the applicable code to AWS(remove ASME) or you can rewrite the WPS to AWS

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 7/15/11, Ramchandra vichare <vicharerke@indiatimes.com> wrote:

From: Ramchandra vichare <vicharerke@indiatimes.com>
Subject: Re: [MW:11737] Clarification of PQR/WPS in FCAW process
To: materials-welding@googlegroups.com
Date: Friday, July 15, 2011, 3:34 PM

Dear friends,

WPS Must be corrected accordingly.
If Welder Qualified in 3G welder can weld 1G&3G position only.(Pl go trhough ASME Sec-IX).
All informations must be fill accordance with formate issued in ASME Sec-IX and not to take shortcut for information because everyone dont know what is what

Regards,
RKVichare.




----- Original Message -----
From: arvinda shan
To: materials-welding@googlegroups.com
Sent: Wed, 13 Jul 2011 19:12:32 +0530 (IST)
Subject: [MW:11723] Clarification of PQR/WPS in FCAW process

Dear Experts,

 

I need some clarification in document review. PQR qualified in FCAW process for 27 mm plate in 3G position. WPS is prepared for structural joint for 34 mm in all positions.What is the essential one?

 


  1. In FCAW proces PQR , Electrode AWS no. E71-T-1C is used. But in WPS E71-T-1 is mentioned. Whether its ok?

  2. PQR in FCAW qualifies 3G position of 27mm plates as per ASME SEc.IX and API-650. What is qualification of position in WPS for 3G whether its ALL POSITION or only 3G postion?

  3. The WPS is to be used for structural activies. ie. as per AWS D1.1. But in WPS also mentioned reference code as ASME sec.IX and AWS D1.1.

Plz clarify.

 

Thanks

 

Arvinda.




--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...