if impact testing is required for the component you need to follow B31.3 requirement also , but you can qualify it as PTC, need not be specified on WPS, however if you want to avoid PTC, then you can specify the limits as 0.5T - T+6mm on WPS)
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
On Wed, Jul 13, 2011 at 4:43 AM, 박종민(PARK, JONG MIN) <carpediem@dsme.co.kr> wrote:
-- Dear Experts
T qualified is specified in ASME Sec. IX QW-451.2 and QW403.6(Max. 2T) and ASME B31.3 Table 323.3.1(0.5T ~ T+6mm).
For piping works for offshore, Shall these two requirements be kept ?
Best regards,
JM
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments