Re: [MW:11675] Poduction impact test

dear sanu,

the impact test is generally mandotary for the low temperature services as at low temperature ( sub zero ) the amount of ductility get reduces & will cause brittle fracture in transition temperature.In order to  ensure the applicable material to use within that temperature  perform an impact test on LOW TEMPERATURE CARBON STEEL.

It is based on your PQR .If your pqr is qualified with the -50 c so you can use same WPS .If not you have to qualify an PQR as essential variable in procedure.( reference asme 9 )

regards

dinesh 

On Mon, Jul 11, 2011 at 11:17 AM, Sanu Krishnan <sanukrishnankutty@gmail.com> wrote:
Dear experts,
       
  Is it Production imact test required for LTCS,upto -50degree C.Already PQR Test qualified in -50 degree C?

--
SANU.K.NAIR
QC INSPECTOR
DAEWOO E & C
ABUDHABI
Ph: 0507464738

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...