Re: [MW:11655] Re: E7018-A1 Electrod

Dear sir
 
The difference between E7018 it contains iron powderd content
 E7018-a1 refers to  chemical composition in asme sec II part c search E-7018-A1 & read out notes point you get the answer of this
only the thing writeen in standatd A-Z refers only chemical composition of electrode
 
pravean
QA/QC welding inspector
ksa
jubail  

2011/7/5 R. Moseley <robert.moseley40@yahoo.com>
Zakaria,
The "A1" designation is for the addition of Chrome moly to the
normally full carbon steel filler metal mixture. It is normally used
for welding/ joining of P3 (Carbon .5Mo materials). In this case it
would not be wise or advisable (as the client has dictated) to use a
filler metal without the addition of the Moly. Hope this helps.

Robert Moseley
Welding Specialist/ Consultant

On Jul 5, 10:11 am, Zakaria ghrab <zakaria.gh...@gmail.com> wrote:
> Hi All,
>
>   In our boiler project we have to weld socket tube A210 Gr A1,  38 mm
> diameter , 4 mm thick  to collector P11 material thick , according client
> WPS we have to weld by E7015-A1.
>
> What's the difference between EXXXX and EXXXX-A1
> May E7018 substitue E7015-A1 ?
>
> Kind regards
>
> --
> *زكرياء غراب
> **GHRAB Zakaria** *
> مسؤول عن الجودة
> QA/QC SENAD
> مشروع المحطة الحرارية ـ الوحدة الرابعة
> المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...