Are the bonders qualified as per code?   In gre the test coupon is subjected to burst test to qualify bonder.
Prior HT check method of statement & HT procedure should include holding time, it shall be min 2 hrs @ 1.5 times n over 1.25 times for next 2 hrs / upto 24 hrs as in gre u can find seepage/ sweating at the joint n again it depends on test location n owner requirements. There may not be a deflection test post fabrication for gre

Cheers,
Srinivas
NKOM-Qatar

Sent from my iPhone 4

On 05-Jul-2011, at 9:41 AM, "k.ilangkumaran ilangkumaran" <k.ilangkumaran@yahoo.com> wrote:

Dear experts,
 
            Kindly share your experiences of above test. What is deflection test and when is it performed? I am witnessing GRE piping installation and what are the documents required prior to test? Is it performed before hydro test or after? How do we accept incase of deviations? Should I insist to provide method of statement from the contractor?
 
Regards
Ilangkumaran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...