it is required based on MDMT (Minimum Design Metal Temp) and thickness, check with your designer whether base material requires impact testing?
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
if your governing code is ASME B31.3 check para 323.2.2 and table 323.2.2
-- On Fri, Jul 1, 2011 at 8:02 PM, lassaad mokrani <lassaad.mokrani@gmail.com> wrote:
Dear Experts,Is impact test required by ASME (in PQR) or only by service conditions for 2" A106 Gr B pipe works???Best Regards,
--
Meilleures salutations
Mokrani Lassaad
00216 20 649 755
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments