[MW:11848] POST WELD HEAT TREATEMENT OF API 2W GR 50/API 2MT1 PIPES WITH THK 3''

Hello Gents,

Using AWS D1.1 as project code, is it wise/Professional to carry out

PWHT on joints made from (TMCP PLATES- API 2W Gr 50/ API 2MT1 Gr 50 rolled into pipes with thickness 3’’)

Used for TKY joints on jackets.

Note: TMCP - thermo-mechanical control process.

Regards

Philip Taiye

Principal QA/QC Welding Engineer

(EPCM-1 Quality Assurance/Control)

DeltaAfrik Engineering Limited

2nd Floor, City Express Bank Building

Plot 1637 Adetokunbo Ademola Street

Victoria Island, Lagos  Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418

e-mail: taiye.philip@worleyparsons.com

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...