Friday, July 8, 2011

[MW:11622] What structure in HAZ


Dear All,

laser cladding of martensitic stainless steel on medium carbon steel .
what micro structure we ll get in HAZ, and is it prone of crack sensitivity??

And, what is weldment shelling out means?(  why chromium carbide forms at the interface of the weld? )

Thank you

Chandu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...