Hi experts,
I would like to clear a point regarding the welder qualification in 6GR position. When the welder qualification test is carried out in 6GR position the ID of the pipe (6"x16mm is welded to 6"x22 mm with plate restriction as per Fig. 4.27 AWS D1.1) is offset. When the test pieces are prepared for bend test is it required to skim the root (offset) section by removing the offset or left as welded and carry out the bend test?
Kind regards,
Martin.
I would like to clear a point regarding the welder qualification in 6GR position. When the welder qualification test is carried out in 6GR position the ID of the pipe (6"x16mm is welded to 6"x22 mm with plate restriction as per Fig. 4.27 AWS D1.1) is offset. When the test pieces are prepared for bend test is it required to skim the root (offset) section by removing the offset or left as welded and carry out the bend test?
Kind regards,
Martin.