Hi All,
In our boiler project we have to weld socket tube A210 Gr A1, 38 mm diameter , 4 mm thick to collector P11 material thick , according client WPS we have to weld by E7015-A1.
What's the difference between EXXXX and EXXXX-A1
May E7018 substitue E7015-A1 ?
Kind regards
--
-- In our boiler project we have to weld socket tube A210 Gr A1, 38 mm diameter , 4 mm thick to collector P11 material thick , according client WPS we have to weld by E7015-A1.
What's the difference between EXXXX and EXXXX-A1
May E7018 substitue E7015-A1 ?
Kind regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments