Wednesday, May 18, 2011

Re: [MW:11088] backing strips

yes i used ceramic backing strip for butt weld joint for 3mm sheet welding. by using ceramic backing strip u dont requre back chipping and back purging so it will save ur time and cost and gives full penetration at bach side.

On Thu, May 12, 2011 at 3:43 PM, ELAMARAN RAJAN <elams.rajan@gmail.com> wrote:
Dear experts

There is any one used removable backing strip for stainless steel butt
welding with out purging
and pls let me know it is really work out as a cost wise and quality wise



--
maran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks and Regards

Ashish  Chauhan
ME-Welding Technology
MSU-Baroda

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...