i think spacer ring is st. st rings used for maintain gap in socket welds pls. correct me if wrong
Mob. 0103955198
From: Hafiz Ali Alvi <alimalvi300@hotmail.com>
To: materials-welding@googlegroups.com
Sent: Mon, May 9, 2011 7:50:31 AM
Subject: RE: [MW:11002] spacer rings
Dear Ilangkumaran,
Regards.
Date: Sat, 7 May 2011 21:57:43 -0700
From: k.ilangkumaran@yahoo.com
Subject: [MW:10996] spacer rings
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Best regards
Ashraf Aly
Mob. 0103955198
From: Hafiz Ali Alvi <alimalvi300@hotmail.com>
To: materials-welding@googlegroups.com
Sent: Mon, May 9, 2011 7:50:31 AM
Subject: RE: [MW:11002] spacer rings
Dear Ilangkumaran,
Are you talking about spade and spacer or spacer bleed ring?
Regards.
Date: Sat, 7 May 2011 21:57:43 -0700
From: k.ilangkumaran@yahoo.com
Subject: [MW:10996] spacer rings
To: materials-welding@googlegroups.com
Dear experts, Can anybody explain me what is spacer ring?Why does it required? Where do se use them? Type of spacer rings etc,. if possible is there any international codes? Thanks in advance. Regards Ilangkumaran |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments: