RE: [MW:10975] RE: 10970] heat input calculation

what is 60 (V*I*60) in this formula?
 

From: vinod.kataria@blissanand.com
To: materials-welding@googlegroups.com
Subject: [MW:10974] RE: 10970] heat input calculation
Date: Fri, 6 May 2011 13:00:05 +0530

You can calculate by using following formula:-

 

Heat Input = (V*I*60)/(Travel Speed in mm) this will come in J for KJ please further devide it with 1000.

 

For the below value the Heat Input shall be

0.50 KJ.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Martin Prad
Sent: Friday, May 06, 2011 11:00 AM
To: materials-welding@googlegroups.com
Subject: [MW:10970] heat input calculation

 

gents,
 
how to calculate the heat input in KJ/mm if i have got the folowing parameters?
 
Amperage=71
Voltage=9.5
Travel speed=3.2 inch/minute
can you please put these in the formula?
 
thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...