Re: [MW:10949] AWS D1.1 WPS M.no changes requiring requalification or not?

Yes

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 5/4/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

From: Srinivas Engr <srinivas.gmsrini@gmail.com>
Subject: [MW:10934] AWS D1.1 WPS M.no changes requiring requalification or not?
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, May 4, 2011, 1:08 AM

Dear all,

as per table 4.5 essential variables..
in base metal, it says to refer table 4.8.
In table 4.8 it says about only group number.
if group number changes from one which is not qualified require
requalification.. ok.
My question is..
Its doesn't says about M.number. so m.no changes is not required
requalification of wps.
can we go with same WPS if g.no mets?
The above said is right or wrong..
clear me.

Reagrds
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...