Dear All, 

i think you can use some manufacturer recommended thinner to clean the serration area.

Thanks & Regards,

Saravanan P P

On Sat, Apr 30, 2011 at 5:57 PM, Adi <adinraos@gmail.com> wrote:
Hi all....

Mistakenly flange serration area painted,
Is anybody having repair procedure for this? It is acceptable to
remove painted flange serration area by wire brush.

Adi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Saravanan  P P
QA/QC Engineer,
Arun Fabricators,
LPG Terminal - HPCL,
HP Petro Park,
Visakhapatnam - 530 009 (A.P)
M - 8008202828.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...