Re: [MW:10911] QW-404.6 of sec IX

Dear Mr Kannayan,
 
               That  is QW 404.6 of sec IX. I regret for inconvenience caused any.
 
Regards
Ilangkumaran


--- On Sun, 5/1/11, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:

From: kannayeram gnanapandithan <kgpandithan@gmail.com>
Subject: Re: [MW:10903] QW-404.6 of sec IX
To: materials-welding@googlegroups.com
Date: Sunday, May 1, 2011, 5:04 PM

QW 406.6 comes under Preheat

On Sat, Apr 30, 2011 at 3:58 PM, k.ilangkumaran ilangkumaran <k.ilangkumaran@yahoo.com> wrote:
Dear experts,
 
               I have checked all the tables in sec IX; no where mentioned QW-406.6 as essential variable or essential variable.
 
        But in page 69 in sec IX it states that A change in nominal size of electrode or diameter specified in the WPS. I couldn't understand this statement. Can somebody explain me please?
 
Regards
Ilangkumaran
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...