Sunday, May 1, 2011

Re: [MW:10909] Hydrotest-API 650

Re-Hydro test should be done.
 
Regards,
 
Sohaib


From: DHANASEKARAN SUBRAMANIAM <subramaniamdhanasekaran7@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, May 1, 2011 8:40:39 AM
Subject: [MW:10902] Hydrotest-API 650

Gents,
After the completion of a tank hydro test, some temporary attachment welding has been made on the shell and roof plates.
What action needs to be taken at this stage, kindly provide the action plan with code references.
 
 
Your Immediate response is highly appreciated.
 
 


--
WITH REGARDS,
DHANASEKARAN .S ,
Mob.no: +96893220429.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...