Re: [MW:10906] Diameter of electrode-reg

He can go one above and one below.if he is qualified in 3.15 mm can weld 4.0 mm and 2.5 mm.

On Sat, Apr 30, 2011 at 3:22 PM, k.ilangkumaran ilangkumaran <k.ilangkumaran@yahoo.com> wrote:
Dear Experts,
 
               While my routine inspection of welding I have noticed Diameter of the electrode used for the capping was not as per the qualified WPS and I was told the diameter of the electrode is not an essential variables.
 
  WPS for SMAW
 
Now as per the sec IX; Table QW-253
 
1) the essential variable QW-404.30
 
2) Supplementary variables QW-404.7/.12
 
3)  Non essential varaiable QW-404.6
 
       &
as per the QW-353
 
1) QW-404.15/.30 were the essential variables for welder qualification.
 
So if the diameter of electrode used in production welds beyond 6mm then only the WPS
needs to be re written? or Should we insist the welder to use what ever mentioned in the qualified WPS? or the welder should use the electrode that he used while performing his WQT.
Can somebody expain me in details how to deal this?
 
Regards
Ilangkumaran
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...