Thursday, May 19, 2011

[MW:11096] Clarification for Dissilmilar Weld Radiography Interpretation

Dear All,
 
Code: ASME Sec VIII, Div 1, Ed'09
Ref:    Base Material - SA 516 Gr.70N, 30 thk , Clad Material - Incoloy 825, 3 mm thk
 
Query:
Material 1: Carbon Steel, Material 2: Composit Material(CS+Incoloy), SA 265
How can we have a good judgement on RT Interpretation for Dissmilar Weld joint as density will vary due to different composition?
Do we have Image Quality Indicator for Dissimilar Metal?
 
Hope to see response from all Sections as usual.
 
Thanks & Regards
Vino-Doha

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...