Wednesday, May 18, 2011

[MW:11085] RE: 11080] SA-213 Gr.T91

Appears to be an error.  All UNS K90901 (“91” alloy) were to be changed to P-No. 15E with publishing of 2009 Edition. 

 

Use P-No. 15E

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of srinivasu
Sent: Wednesday, May 18, 2011 4:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:11080] SA-213 Gr.T91

 

Dear Experts

 

What's the P.No. of Material Specification of SA-213 Gr.T91?

 

I refer Sec.IX 2010 Edition as per QW-422 - it's P.No.5B Gr.No.2

                                         as per Appendices-D - it's mentioned P.No.15E Gr.No.1

 

Which one is the correct?      

 

 

With Regards

 

 

Srinivasu V

Welding Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments: