Wednesday, May 4, 2011

[MW:10941] SS316L PWHT

Dear All,
We are fabricating two vessels in SS316L (thickness 12mm) diameter
794mm each to be used as fuel gas separators. We have tried to
convince our client that we don't need any PWHT for the shell, since
the strain doesn't exceed 5% and that NACE MR0175 doesn' oblige that.
We decided to make the PWHT only for the dish ends.
But our client insisted to do it anyway for the whole vessels.
I need your input urgently

Best Regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...