dear experts,

pl guide me that how to select filler wire according to given material.for instance if material is dissimilar, base material having 9Cr,1Mo,other material SA 351 HK 40,having Cr.23-27,Ni.19-22.one of our expert suggested that ErNiCr-3 as a filler wire.Other than material what characteristics are we have to take in to consideration to select filler wire.
 

thanks & regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...