It depends on the applicable code requirement.
For ASME sec VIII Div.2 2 please refer to table 3.13 of part 3 part where the minimum impact values also depend on the parameter as well as sec. VIII div.1 (specified minimum yield strength and thickness of the material)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
For ASME sec VIII Div.1 please refer to fig. UG-84.1 where the impact value is depend on minimum specified yield strength of the material and the maximum nominal thickness.
For ASME sec VIII Div.2 2 please refer to table 3.13 of part 3 part where the minimum impact values also depend on the parameter as well as sec. VIII div.1 (specified minimum yield strength and thickness of the material)
On Tue, Apr 19, 2011 at 8:26 PM, senins welo <senins054@gmail.com> wrote:
--dears,how can find the impact value of material using any code ,please explain.thank u
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments