Friday, April 15, 2011

RE: [MW:10684] stainless steel Grade 321H Weldability

ER 347 is compatible fillet metal for this grade

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 15, 2011 3:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:10683] stainless steel Grade 321H Weldability

 

Hi all,

  In our project we have to weld Austenetic SS grade 321H full GTAW, we used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is it true ? use ER 308 is not compatible with these grade ?

Please help me


Regards



No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...