Re: [MW:10604] radiography of longseam by panaromic method

Hello Azmi
 
There's no such thing as panoramic shot on the long seam, it only applies to circ seams. As per my Level III, you only need one penny per shot but it's good practice to have one on both ends and on in the middle, If you don't agree to it, check the density of all the films and see whether it complies with the code re variance of density.
 
Ricardo

On Mon, Apr 4, 2011 at 11:19 AM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
contractor has carried out radiography of the longseam of a vessel in one shot by panaromic method inspite of doing RT by sinlgle exposure method of each segment of the longseam.
 
while reveiwing RT films it was observed that few films for the longseam are not having penetrameter image on them.
 
kindly inform me whether it is acceptable to do RT of longseam by panaromic method and joint can be accepted with  few films not having penetrameter image  on them. 
 
Construction code for the vessel is ASME SEC VIII DIV 1.
 
Thanks in advance for your valuable suggestions.
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...