Dear Friends
I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.
I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.
However the Izod testing temperature is not mentioned.
Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.
Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9769316004
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.
I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.
However the Izod testing temperature is not mentioned.
Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.
Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9769316004
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments