[MW:10592] radiography of longseam by panaromic method

Dear All,
 
Greetings.
 
contractor has carried out radiography of the longseam of a vessel in one shot by panaromic method inspite of doing RT by sinlgle exposure method of each segment of the longseam.
 
while reveiwing RT films it was observed that few films for the longseam are not having penetrameter image on them.
 
kindly inform me whether it is acceptable to do RT of longseam by panaromic method and joint can be accepted with  few films not having penetrameter image  on them. 
 
Construction code for the vessel is ASME SEC VIII DIV 1.
 
Thanks in advance for your valuable suggestions.
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...