On Wed, Mar 16, 2011 at 7:05 AM, pgoswami <pgoswami@quickclic.net> wrote:
 
Hello VPV,
 
Stellite 6 alloy is a common material for valve seats  both for sour and non sour services. S.S 316 is not the exact replacement for Stellite. 316 S.S basically lacks the strength and hardness which is required in a valve seat to avoid galling and erosion. Any one of those can cause "passing of valves".
 
Please look in MR-0175 -part -3 on the acceptance of Co alloys for sour services.
 
Should you be interested I may forward you some more information  which I have.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vino Varghese
Sent: Tuesday, March 15, 2011 5:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:10362] Which is better material for Seat / Control Valves / Sour Service

Dear Experts,
 
The Data sheet for Control Valve calls for Seat Material of Trim as Stellite 6 + ENP and Supplier is offering SS 316.
Whis is better - Is it Stellite 6 + ENP or SS 316?
 
Info: Service to be used is Sour Service.
Temperature : 60 Degree Centrigrade
Inlet Presure: Max. 0.5 bar g
Otlet Presure: Max. 0.3 bar g
 
Appreciate to see response ASAP.
 
Regards
VPV

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...