Skip to main content

Re: [MW:10366] Basic Question

Where is SB, SC, SD?   Correct me if i am wrong....
 
There is ASME sec II, Part A (not section A), Part B (not section B), Part C, (not section C), Part D (not section D)
 
For Specs with SB 209, same like SA. That is ASTM standards adopted by ASME..
 
Part B for non ferrous materials
 
Part C - Welding consumables
 
Part D - Stress values
 
Thanks
 
murugesan
 
 


 
On Tue, Mar 15, 2011 at 1:24 PM, Harish Kannepalli <harishkannepalli@gmail.com> wrote:
Dear Mr Murugesan,
                            Then what is SB, SC & SD in ASME, where some are developed entirely by ASME. Please explain.

2011/3/14 murugesan jeyaraman <jmurugesan@gmail.com>
Hi
 
SA does not mean Section " A"  It is a wrong understanding.
 
There is a standard called ASTM International (ASTM),  known as the American Society for Testing and Materials.
It is an  international standards organization that develops and publishes technical standards for a wide range of materials, products, systems. For example A106, A105, A517 and etc...
 
Here, " A " refers it is ASTM standard, and the number 106, 105, 517 are the designation given to particular type of materials, like  naming that pariticular product with some numbering convention.
 
A 106 - Covers seamless carbon steel pipe for High temperature service
 
A 516 - cover carbon steel plates for High temperature service
 
Refer ASME sec II part A for details about this specifications.
 
Now comes to "SA"  - ASME adopts the above ASTM standard and rename the designation by  putting "SA" to same ASTM standards numbers. now it is called SA106, SA 516 and so on... for your case SA 387 This is spec for  pressure vessel plates of Chromium-Molybdenum
 
Gr-22    This refers to Grade of materials within that specification, There various grades like GR11, Gr 22, Gr 91 , Gr 5, Gr 9 and so on- this classified based on cromium content,
 
Class -2 - Above Gr 22, 22, 9, 91 materials further categorised as class 1 and class 2 based on Mechanical properties(Tensile and Yield strength)
 
B3 - alloying charactersitics for Gr 22 materials (2 1/4 chrome  1 Moly).
 
Piece of advise: You are in learning stage, you have to study more codes and standards, If you are working in a ASME accredited workshop or in a workshop that do  Boiler pressure parts, you will learn a lot ....
 
Or there are lot of online guides, please refer to those guides for basics, you read yourself from codes and standards.
 
Thanks
 
Murugesan
 
 
 
On Sat, Mar 12, 2011 at 8:03 PM, <fire_praves@indiatimes.com> wrote:
Dear Sir s

As I am a novice, please help in some basics

I have come across a material of Specification
SA 387 Gr22 Class 2

Please tell me what is denoted by 387, Gr 22 and Class 2.
Do these figures have any thing to do with strength or chemical composition?

Also for welding this material to a material of same specification, E9018 B3 is mentioned.

Please tell me what is denoted by B3?


Regards,
prv

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...