Dear Elias,
I had an experience replacing whole bottom plate. The standard used is API 653 (Tank Inspection, Repair, Alteration, and Reconstruction).
I did oil leak test for the bottom corner welding, vacuum box test for bottom plates welding, and finally hydrostatic test.
Please refer to API 653 for the minimum requirement.
Best Regards
Prihandoko
Truba Jaya Engineering
--
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I had an experience replacing whole bottom plate. The standard used is API 653 (Tank Inspection, Repair, Alteration, and Reconstruction).
I did oil leak test for the bottom corner welding, vacuum box test for bottom plates welding, and finally hydrostatic test.
Please refer to API 653 for the minimum requirement.
Best Regards
Prihandoko
Truba Jaya Engineering
Powered by Telkomsel BlackBerry®
From: Ahmed Elias <alyassahmed@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Sat, 12 Mar 2011 13:46:51 +0300
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:10292] Existing Tank
hi Dear,
You Have to do hydrostatic test
regards
On Fri, Mar 11, 2011 at 3:29 PM, srinu p <sree.dream6@gmail.com> wrote:
Dear All,We have two existing tanks ( 20 years old) 3 mtrs height and 5.7 mtrs dia.. Bottom plate thickness - 8 mm.As per client requirement we have shift the tanks to another place and also they want to change the Bottom plate.1. As per API standard or any other standards, if we change the bottom plate, which type tests are required for bottom plate inspection. My opinion is Vaccum Box and DPI or MPI tests are enough? or Any other tests are required?2.And also if we are using same bottom plate UT thickness guage checking and VB, DPI/MPI tests are enough? Is it acceptable?Please share your experience.regards,P.Srinu--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
AHMED MUHAMMAD ELIAS
MECHANICAL ENGINEER
MECHANICAL ENGINEER
ASNT LEVEL II NDT INSPECTOR
IRAQ :-+9647710951885,+9647503136603
PLEAS FEEL FREE TO CONTACT ME FOR ANY INQUIRY
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments