Dear Sampath

Check your PQR for following

Grade of material used
thickness
Filler wire & its grade
Pre heat & Post Heat
Proces/Position
Check all the parameters am meeting the rules( your consumable grade
should match your material)
Check all tests are conducted asper the code
Review your WPS for
applicable grades of material
applicable thickness( considering PQR thickness & Pre heat temp)
range of position


All these you have to check as per the code on which you working( ASME,GL.DNV..)


Thanks & Regads
Samshuddin.K
Bharati Shipyard Ltd


On Thu, Mar 10, 2011 at 9:07 AM, Sampath Kumar <skthatham@gmail.com> wrote:view
> Dear Friends,
>
> It is great to note that those who write to this group are getting their
> doubts cleared in the subject plus they gain more knowledge by subscribing
> to this group.That made me to send me this request.
> Can anyone may please guide me how to review WPS and PQR,in a very simple
> way.
> Thanking You all
> With Best Regards
> sampath
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...