Hi
Yes you are right but it is only applicable for Thickness of Weld Metal Qualified with minimum of three layers.
--
With Warm Regards,
Prakash Verma
Metallurgist-Drilling Riser Systems
QS Supply Chain.
Aker Solutions Supply chain hub-India
AkerSolutions
Tel.+91-20-66 28 8538
Email. prakash.verma@akersolutions.com
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Wednesday, March 09, 2011 10:44 PM
To: materials-welding@googlegroups.com
Subject: [MW:10246] ASME IX - Welder's qualification Thickness range
Hi all,
As per ASME sect IX table QW-452-1(b), for welder's qualified in test coupon thickness greater or equal than 13 mm, he's will be qualified to wed thickness " Maximum to be welded"
May my interpretation is true ??
In this case, Can i qualify all welder's in 13 mm thickness, he will be qualified for all thick ( PWHT is not essential variable for welders) and cover all thickness range ?
Regards
--
-- As per ASME sect IX table QW-452-1(b), for welder's qualified in test coupon thickness greater or equal than 13 mm, he's will be qualified to wed thickness " Maximum to be welded"
May my interpretation is true ??
In this case, Can i qualify all welder's in 13 mm thickness, he will be qualified for all thick ( PWHT is not essential variable for welders) and cover all thickness range ?
Regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.
Comments