Dear Mr.Anand...
 
Below clarification is from my experience..
 
Most of the time during valve testing shell and back seat hydro will be carried out in single setup.. Some times if you advise them to open the valve 100 % then every chances for the back seat bush to push against the packing area which may mask the back seat leak..
 
hence it is preferable to have partial opening of the valve.
 
br,
msms

On Sun, Mar 6, 2011 at 12:26 PM, rockers Anand <razrockers@gmail.com> wrote:

Dear All,

Kindly give the exact reason for why the valves 90% opened during hydrostatic test of piping? And why it is not opened 100%?

Anand.M




















--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...