ST 37.2 is an equivalent of BS EN 10025 Gr. S235 steel with the minimum Y.S. 235 mPa.
regards,
Date: Wed, 2 Mar 2011 17:48:19 +0530
Subject: [MW:10101] Fwd: st 37-2
From: pkgamne@gmail.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
regards,
Cold formed sections
Mechanical properties according to EN 10249-1:1995 and corresponding former national standards. Other steel grades can be delivered on request.| Standard referred to: EN 10249-1:1995 | Former references | ||||||
|---|---|---|---|---|---|---|---|
| Steel grade | Minimum yield strength ReH | Minimum Tensile strength Rm | Minimum elongation | F | D | GB | B |
| N/mm2 | N/mm2 | % | |||||
| S 235 JRC | 235 | 340-470 | 26 | E 24-2 | St 37.2 | 40 B | AE 235-B |
| S 275 JRC | 275 | 410-560 | 22 | E 28-2 | St 44.2 | 43 B | AE 275-B |
| S 355 JOC | 355 | 490-630 | 22 | E 36-3 | St 52.3 U | 50 C | AE 355-C |
The C in JRC and J0C stands for cold forming aptitude according to EN 10025:1993.
Date: Wed, 2 Mar 2011 17:48:19 +0530
Subject: [MW:10101] Fwd: st 37-2
From: pkgamne@gmail.com
To: materials-welding@googlegroups.com
Dear All
Any body Can tell me equivalent grade for st-32 grade material.
Thanks in advance.
regards
Prayag
Nasik
India
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments