Dear Sir,

We have run PQRas per AWS D 1.1 -2010 n API 5 L Grade X - 65 PSL 2, Pipe OD 1219mmwall thickness 22mm. Position 6G, process SMAW welded by 2 welders.

 RT - Gamaray Iridium 192 used  for RT
One Slag inclusion of length 40mm ie. at Top observed.

Now RT is failed , so PQR is failed again to run PQR that way our third party is saying. Other segments are ok and accepted.

I have some questions in my mind that is such a large dia pipe we carried out PQR, instead of wasting time and money , whether it is possible to carryout the mechanical testing by leaving the slag portion and requalifying the welder as slag has come? 

If there is any applicable clause  with in the code or any acceptable methods and ways please tell experts with supporting document evidence.



Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P

Senior Manager QA/QC
AFCONS Infrastructure Ltd
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...