Hi,

 

As per my View, Distance between two circumferential welding will be equalant to D – diameter.

 

Many other friends had suggested for less than that also, but if the distance is “D”, then it will be easy for fitup and all, then after any RT is also easy.

 

 

Thanks & Regards

 

Lakshman kumar.B | Manager - QA/QC | LANCO  INFRATECH LIMITED
Plot# 1255 | Sanjeevani Chowk | Mahanadi Vihar | Cuttack 753004

Phone : + 91-671-2445033| Mobile: +91 9937286851 | www.lancogroup.com

Go Green |The future will thank you

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, February 18, 2011 3:51 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9924] min. distance between two circumferential welds

 

Hi,

i have same problem in last project, power piping process .According B31.1, we don't found information,  we get approbation from engineering.

2011/2/18 shankar k <shankark.qc@gmail.com>

hi,

can anybody exlain what is the distance between two circumferential butt joints ?  we are welding 5" pipeline joints of A53 Gr.B

 

shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...