Friday, February 18, 2011

Re: [MW:9934] Radiography

RT-3
 
Category A,B,C& D joints with Joint Efficiency of 1.00 or 0.85 - Spot Radiography
 
Spot Radiography - One Radiography Spot for 15 metre of weld
 
RT-4
 
Where no markings is specified or part of the Vessel radiographed


J.GERALD JAYAKUMAR
00919344954677
 


--- On Thu, 2/17/11, Azhar Ali <aab51214@yahoo.com> wrote:

From: Azhar Ali <aab51214@yahoo.com>
Subject: [MW:9918] Radiography
To: materials-welding@googlegroups.com
Cc: azali@olayandescon.com
Date: Thursday, February 17, 2011, 7:01 PM

Anybody  can describe the RT1.RT2.RT3.RT4 in an easy way.
 
Regards
azali
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...