RT-1
Long Seam (A), Circum Seam(B), Nozzle to Flange(C) & Nozzle to Shell/DE(D) category Joint - Full Radiography for thickness above
38 mm - Carbon steels(P1)
19mm - LAS (P3)
16mm - LAS (P4)
0 mm - LAS (P5A,5B&5C)
For Stainless steel & Non-ferrous refer particular sections of Code.
 
Exception to the Above :
1. Category B & C butt welds associated with Nozzles & communicating Chambers that neither exceeds NPS 10 nor 29 mm Wall thickness
2. Category D Joint forming an Corner weld instead of LIP Butt welds.
 
RT-2
 
Category A & D Butt welds - Full Radiography
Category B&C Joint where intersects with Category A joint in Shell/DE - Spot radiography
 
RT-3
 
 
J.GERALD JAYAKUMAR
00919344954677
 


--- On Thu, 2/17/11, Azhar Ali <aab51214@yahoo.com> wrote:

From: Azhar Ali <aab51214@yahoo.com>
Subject: [MW:9918] Radiography
To: materials-welding@googlegroups.com
Cc: azali@olayandescon.com
Date: Thursday, February 17, 2011, 7:01 PM

Anybody  can describe the RT1.RT2.RT3.RT4 in an easy way.
 
Regards
azali
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...