Re: [MW:9932] Corten & carbon Steel weldability

Dear mr. zakaria,

As already explain by mr. Muthu corten is unspecified material by asme thuswps/ pqr qualified for corten shall only be used to weld corten mtrl. U can't mixed with carbon steel since it is fall under p1 thus u need to qualify a new wps for ur c steel. Please correct me if I'm wrong.

Brgds
AW
From: Zakaria ghrab <zakaria.ghrab@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Fri, 18 Feb 2011 10:13:30 +0000
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Cc: muthusrinivasan muthuselvam<msms2k@gmail.com>
Subject: Re: [MW:9925] Corten & carbon Steel weldability

Hi,

   My request is : May Corten PQR qualify Carbon steels WPS and how we can approuv it from ASME IX ?

Regards

2011/2/18 muthusrinivasan muthuselvam <msms2k@gmail.com>
Dear Mr.Zakaria..
 
Corten is unspecified material as per ASME... you can say that as unassigned and preferred electrode is E 7018 W -made to order.
 
I hope this is for chimney or some container..
 
br,
 
msms

On Thu, Feb 17, 2011 at 9:14 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  I need to know the P number of corten steels, i have on PQR according ASME sect IX corten to corten, i need to use it to prepare WPS for Carbon steels but i have doute Corten is PN°1 or PN°3, serashing in internet : Equivalent Corten is ASTM SA 242, is it true?
--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...