Re: [MW:9926] min. distance between two circumferential welds

 

 Hi,

Considering the heat affected zone , It has been fixed as a thumb rule  4times of pipe thickness .

There are no specific code  as for as my knowledge. 

 

 

With regards

 

 

T.Mahendran,

Tabouk - KSA,


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, February 18, 2011 1:21:15 PM
Subject: Re: [MW:9924] min. distance between two circumferential welds

Hi,

i have same problem in last project, power piping process .According B31.1, we don't found information,  we get approbation from engineering.

2011/2/18 shankar k <shankark.qc@gmail.com>
hi,
can anybody exlain what is the distance between two circumferential butt joints ?  we are welding 5" pipeline joints of A53 Gr.B
 
shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...