Hi,

   My request is : May Corten PQR qualify Carbon steels WPS and how we can approuv it from ASME IX ?

Regards

2011/2/18 muthusrinivasan muthuselvam <msms2k@gmail.com>
Dear Mr.Zakaria..
 
Corten is unspecified material as per ASME... you can say that as unassigned and preferred electrode is E 7018 W -made to order.
 
I hope this is for chimney or some container..
 
br,
 
msms

On Thu, Feb 17, 2011 at 9:14 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  I need to know the P number of corten steels, i have on PQR according ASME sect IX corten to corten, i need to use it to prepare WPS for Carbon steels but i have doute Corten is PN°1 or PN°3, serashing in internet : Equivalent Corten is ASTM SA 242, is it true?
--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...