Friday, February 18, 2011

Re: [MW:9919] Corten & carbon Steel weldability

Dear,
P no 1 and equivalent SA 242 for welding choose SFA 5.29 W cu content wire In FCAW.(E81T1W2)
Regards
Pradeep


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 17 February, 2011 9:14:27 PM
Subject: [MW:9916] Corten & carbon Steel weldability

Hi all,

  I need to know the P number of corten steels, i have on PQR according ASME sect IX corten to corten, i need to use it to prepare WPS for Carbon steels but i have doute Corten is PN°1 or PN°3, serashing in internet : Equivalent Corten is ASTM SA 242, is it true?
--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...