You can use either ER 308 or ER 316.
 
For low carbon L grade of Base material, you can use the L grade of electrode/Filler Rod.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Thu, 2/17/11, Abhonkar, Abhay (NAR) <AAbhonkar@Dresser-Rand.com> wrote:

From: Abhonkar, Abhay (NAR) <AAbhonkar@Dresser-Rand.com>
Subject: [MW:9914] welding of dissimilar material
To: materials-welding@googlegroups.com
Date: Thursday, February 17, 2011, 10:37 AM

Dear Sir,

We want to weld SS 304 pipe with fittings made of SS 316.

Request you to suggest the suitable filler wire for GTAW process.

 

Also from where (ASME or B31.3) I can select the reference document

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...