Re: [MW:9912] Minimum shell width

ASME Sec.VIII Div.I doesn't restricts on the width of the shell. Normally it will be 3 or 4 meters. Also depends on your requirement.
 
Only thing you need to taker care is the distance between weld seams and also nozzle welds. A gap of 100mm or 2t is required.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Wed, 2/16/11, mahesh patel <maheshpatel079@yahoo.com> wrote:

From: mahesh patel <maheshpatel079@yahoo.com>
Subject: [MW:9901] Minimum shell width
To: materials-welding@googlegroups.com
Date: Wednesday, February 16, 2011, 7:30 AM

Dear all

Pl advise me minimum width of shell from plate i can take as per ASME SEC VIII Div-1?

Can i take 300 mm width shell from plate?


Please suggest me.

Regards

Mahesh Patel

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...