Re: [MW:9911] Info on weld failure path analysis

Check ASME Section VIII Div 1 UG 41 for nozzle weld strength/failure paths.
Sample calculations are in Appendix-L., 7.2, to 7.8

Arun
On Wed, Feb 16, 2011 at 5:02 PM, betsforall <betsforall@rediffmail.com> wrote:
Dear Colleagues

I would like to what is a weld failure path analysis and why should it be performed. if some one have some details of how to perform the WFPA or some reference material, request you to please share the same.

Best Regards.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...