Monday, February 14, 2011

Re: [MW:9861] I.Q.I

Yes, steel need to be used (FE) IQI exsample 10-FE-EN
Other metaerial Cu = Copper, Ti=Titan, Al=Aluminium.
FE is for all ferrous materials like carbon, Stainless, duplex etc.

regard,
Jimmy


On Mon, Feb 14, 2011 at 12:46 PM, ali asghari <asgharialigl@gmail.com> wrote:
> Dear All
>  for radiography of duplex stainless steel ,the material of I.Q.I must be
> from this type or not according to ASME sec V?
> Grouping of material in SE747 only mention to Carbon steel and seri 300
> stainless steel.
> regards
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...